Pottery Glaze Troubleshooting: Why Is My Glaze Crawling, Crazing, or Bubbling?
    Glazing

    Pottery Glaze Troubleshooting: Why Is My Glaze Crawling, Crazing, or Bubbling?

    April 30, 2025•4 min read

    Glazing is one of the most exciting (and unpredictable) parts of pottery — and it can also be one of the most frustrating. You open the kiln expecting a smooth, glossy surface… and instead find cracks, pinholes, or bare patches.

    If you’ve experienced crawling, crazing, or bubbling, don’t worry — you’re not alone. This guide breaks down the most common glaze issues and how to fix them.


    What Is Glaze Crawling?

    Symptoms: Glaze pulls away from parts of the pot, leaving bald patches.

    Common Causes:

    • The bisque surface was too dusty or oily.
    • The glaze was too thick.
    • The glaze didn’t adhere well due to poor mixing or clay body mismatch.

    How to Fix It:

    • Always clean bisqueware with a damp sponge before glazing.
    • Apply glaze in thin, even coats.
    • Stir and sieve your glaze thoroughly before use.

    What Is Glaze Crazing?

    Symptoms: Fine, hairline cracks all over the glaze surface.

    Common Causes:

    • The glaze shrinks more than the clay as it cools.
    • Clay and glaze are not well matched for expansion/contraction rates.

    How to Fix It:

    • Choose a glaze better suited to your clay body.
    • Try adjusting the glaze recipe (e.g., lower silica or add alumina).
    • Bisque fire slightly higher to mature the clay more fully.

    Note: Some potters love the look of crazing and use it intentionally — but for functional pottery, it can harbor bacteria and weaken the piece.


    What Is Glaze Bubbling (or Pinholing)?

    Symptoms: Tiny holes, bumps, or craters in the glaze surface — like acne on your pot.

    Common Causes:

    • Gases escaping from the clay during firing.
    • Firing too fast, especially in the early stages.
    • Glaze applied too thickly.

    How to Fix It:

    • Slow down the firing schedule, especially around 1,000–1,500°F.
    • Ensure bisqueware is clean and fully dry before glazing.
    • Consider reformulating your glaze to better flow at peak temp.

    Quick Troubleshooting Chart

    | Issue | Most Common Cause | Quick Fix | |------------|------------------------------|-----------| | Crawling | Dirty bisque or thick glaze | Clean surface, thin coats | | Crazing | Clay-glaze mismatch | Adjust glaze or switch clay | | Bubbling | Fast firing or gas escape | Slow firing, thinner glaze |


    Keep a Glaze Journal

    Document your firing schedules, clay body, glaze recipe, and any weird results. Over time, patterns will emerge — and Terrasate can help you track all of it in one easy place.


    Final Thoughts

    Every potter runs into glaze problems — it’s part of the process. Use mistakes as learning opportunities, and don't be afraid to experiment. You'll be amazed how much more consistent your results become once you know what to look for.

    Happy glazing!